◆Incoloy800H (Ns112/N08810), I-Incoloy800HT, Incoloy800 (Ns111/N08800) zizinto ezintathu ezizezohlobo olufanayo lwe-nickel-iron-chromium alloy series, zinokumelana ne-corrosion, ukumelana nokunyuka kunye nobushushu obuphezulu bokumelana ne-oxidation. unyango Izixhobo zokufakela, izixhobo zokugquma izixhobo zokufudumeza i-alloy tubular, iikhemikhali kunye nezixhobo zokulungisa i-petroleum.
◆Incoloy825 (Ns142/N08825) yi-alloy yobunjineli ngokubanzi.Inokumelana ne-asidi kunye ne-alkali yesinyithi ye-corrosion resistance kuzo zombini i-oxidizing kunye nokunciphisa indawo.Umxholo we-nickel ophezulu wenza ukuba i-alloy ibe nokumelana noxinzelelo lwe-corrosion.Isetyenziswa ngokubanzi kwiinkalo zoshishino ezahlukeneyo apho ubushushu bokusebenza bungekho ngaphezu kwe-550 °C.
◆Incoloy901 yintsimbi yokuqina kwemvula, yintsimbi ekwaziyo ukumelana nobushushu.I-alloy inamandla aphezulu esivuno kunye namandla ahlala ephantsi kwe-650 ° C, ukuxhathisa okulungileyo kwe-oxidation ngaphantsi kwe-760 ° C, kwaye izinzile ukusetyenziswa kwexesha elide.Isetyenziswa kakhulu ekwenziweni kwamalungu anje ngeendawo ezijikajikayo zenqwelo moya kunye neenjini ze turbine zerhasi ezisebenza ngaphantsi kwe 650 °C.
◆Incoloy925 (N09925) yintsimbi ye-alloy enamandla omatshini kunye nokumelana nokugqwala okukhulu.Ihlala isetyenziselwa ukwenziwa kweengxenye kwi-oyile kunye negesi yokomba #izixhobo.
◆ I-Incoloy926 i-austenitic stainless steel ene-chemical composition efana ne-alloy 904L, umxholo wayo we-nitrogen unyuswe malunga ne-0.2%, kwaye umxholo wayo we-molybdenum ngu-6.5%.Isetyenziswa kakhulu kubunjineli baselwandle, kubume begesi ye-asidi, inkqubo ye-flue gas desulfurization.
◆Incoloy20 luhlobo lwezinto zetsimbi ezinokusebenza ixesha elide phantsi kobushushu obuphezulu obungaphantsi kwe-600 ℃ kunye noxinzelelo oluthile.
◆I-Incoloy330 inamandla amakhulu, ukumelana ne-oxidation elungileyo, ukuxhathisa ukubola, ukuxhathisa ukudinwa okulungileyo, ukuqina kwe-fracture kunye nezinye iimpawu, kwaye ifanelekile kumandla enyukliya, imboni yeekhemikhali, kunye nezinye iindawo zoomatshini.
Ukwakhiwa kweekhemikhali
IBanga | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | enye |
akukho mkhulu kune | |||||||||||||
I-Incoloy800 | 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19 ~ 23 | 30 ~ 35 | isiseko | 0.15 ~ 0.6 | 0.15 ~ 0.6 | ≤0.75 | - | - |
I-Incoloy800H | 0.05 ~ 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19 ~ 23 | 30 ~ 35 | isiseko | 0.15 ~ 0.6 | 0.15 ~ 0.6 | ≤0.75 | - | - |
I-Incoloy800HT | 0.06 ~ 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19 ~ 23 | 30 ~ 35 | isiseko | 0.15 ~ 0.6 | 0.15 ~ 0.6 | ≤0.75 | - | Al+Ti 0.85~1.2 |
IKholoyi825 | 0.05 | 0.5 | 1 | 0.03 | 0.03 | 19.5-23.5 | 38-46 | isiseko | ≤0.2 | 0.6-1.2 | 1.5~3 | 2.5–3.5 | - |
I-Incoloy901 | 0.1 | 0.6 | 1 | 0.03 | 0.3 | 11 ~ 14 | 40 - 45 | isiseko | ≤0.35 | 2.35–3.1 | ≤0.5 | 5 ~7 | Co≤1.0 |
IKholoyi925 | 0.03 | 0.5 | 1 | 0.03 | 0.03 | 19.5-23.5 | 42-46 | isiseko | 0.15 ~ 0.5 | 1.9-2.4 | 1.5~3 | 2.5–3.5 | - |
IKholoyi926 | 0.02 | 0.5 | 2 | 0.01 | 0.03 | 19-21 | 24-26 | isiseko | - | - | 0.5 ~ 1.5 | 6 ~7 | N15 ~0.25 |
I-Incoloy020 | 0.1 | 0.8 | 0.5 | 0.013 | 0.013 | 23.5-26.5 | - | 13-16 | ≤1.5 | 0.3-0.7 | ≤0.5 | 2.5–3.7 | - |
IKholoyi330 | 0.04 ~ 0.08 | 1 - 1.5 | 2 | 0.03 | 0.03 | 18 ~ 20 | 34-37 | isiseko | - | - | ≤1 | - | - |
Ubuncinci bepropathi ye-alloy
IBanga | urhulumente | amandla okuqina RmN/m㎡ | Amandla eSivuno Rp0.2N/m㎡ | Elongation As% | Brinell ubulukhuni HB |
I-Incoloy800 | Unyango lwesisombululo | 500 | 210 | 35 | - |
I-Incoloy800H | Unyango lwesisombululo | 450 | 180 | 35 | - |
I-Incoloy800HT | Unyango lwesisombululo | 500 | 210 | 35 | - |
IKholoyi825 | Unyango lwesisombululo | 500 | 220 | 30 | - |
I-Incoloy901 | Unyango lwesisombululo | 900 | 550 | 25 | - |
IKholoyi925 | Unyango lwesisombululo | 650 | 300 | 30 | - |
IKholoyi926 | Unyango lwesisombululo | 650 | 295 | 35 | - |
IKholoyi20 | Unyango lwesisombululo | 700 | 300 | 32 | - |
IKholoyi330 | Unyango lwesisombululo | 750 | 310 | 35 | - |