I-MONEL nickel-copper alloy 400 (UNS N04400) i-alloy-solution alloy enokuthi iqiniswe kuphela ngokusebenza okubandayo.Inamandla aphezulu kunye nokuqina kuluhlu olubanzi lobushushu kunye nokumelana okugqwesileyo kwiindawo ezininzi ezonakalisayo.I-alloy 400 isetyenziswa ngokubanzi kwiinkalo ezininzi, ingakumbi elwandle kunye nokulungiswa kweekhemikhali.Ukusetyenziswa okuqhelekileyo ziivalvu kunye neepompo;impompo kunye ne-propeller shafts;izixhobo zaselwandle kunye nezibophelelo;izinto zombane neze-elektroniki;imithombo;izixhobo zokulungisa imichiza;iitanki zepetroli kunye namanzi amatsha;izixhobo zepetroleum ekrwada, zilungise iinqanawa kunye nemibhobho;izifudumezi zamanzi zebhoyila kunye nezinye izifudumezi zobushushu;kunye nezifudumezi ezidayayo.Ii-Chemical Compositions