I-SUPER DUPLEX S32760 / F55 / 1.4501
INKCAZO
1.Ukubonelela ngamandla aphezulu kunezo zombini i-austenitic kunye ne-22% ye-Cr Duplex Stainless Steels UNS S32760 (F55) ifanelekile kwiintlobo ezahlukeneyo zezicelo kumashishini afana ne-Oil & Gas, i-CPI (i-Chemical Processing Industries), kunye neendawo zaseLwandle.
I-UNS S32760 (F55 / 1.4501) idweliswe kwi-NACE MR 01 75 ngenkonzo emuncu kwaye ifumene imvume ye-ASME yezicelo ze-Pressure Vessel.
amanqanaba amandla ngonyango olulula lobushushu kwiiMeko ze-RH 950 kunye ne-TH 1050. Amandla aphezulu aphezulu e-Condition CH 900 inika iingenelo ezininzi apho u-ductility olinganiselwe kunye nokusebenza kuvumelekile. Kwimeko yayo yonyango lobushushu, le ngxubevange ibonelela ngeempawu ezikhethekileyo zomatshini kumaqondo obushushu ukuya kuma-900 °F (482 °C).
Iphepha leDatha leMathiriyeli
Ingxubevange | Super Duplex S32760 |
Umbandela onguNombolo. | 1.4501 |
EN isimboli (mfutshane) | X2CrNiMoCuWN25-7-4 |
UNS | I-UNS S32760 |
Ileyibhile yomsebenzi obhalisiweyo | I-ASTM A182/ F55 |
Ukuqulunqwa kweekhemikhali
C | Cr | Cu | Fe | Mo | Mn |
% | ≤ % | ≤ % | % | % | |
0.030 ubuninzi | 24 <26 | 0.5<1.0 | Isikhumbuzi | 3.0 <4.0 | 1.0 ubuninzi |
N | Ni | P | S | Si | W |
% | % | % | % | ≤ % | % |
0.20<0.30 | 6.0<8.0 | 0.030 ubuninzi | 0.010 ubuninzi | 0.010 ubuninzi | 0.50<1.0 |
Iipropati eziZodwa
Abaselula iModulus N/mm2 | Uxinaniso kg/dm³: | IMagnetic Permeability |
199 x 10³ | 7.81 g/cm³ | 33 |
Ukuxhathisa okugqwesileyo kwimingxuma kunye nemingxuma / ukukhukuliseka komhlaba
Iinkcukacha
● EN 10088-3 1.4501
● ASTM A473 UNS S32760 Forgings
● ASTM A182 Grade F55 UNS S32760 Forged Flanges
● I-ASTM A240 UNS S32760 Iphepha kunye nePleti
● ASTM A479 UNS S32760 Bar
● I-ASTM A276 UNS S32760 Imeko A
● NACE MR 01-75
Izinto eziphathekayo ziza nesatifikethi se-3.1.
3.2 Izatifikethi ziyafumaneka ngentlawulo eyongezelelweyo.
Iipropati zoomatshini
0.2% Uxinzelelo lobungqina (N/mm2 ) [ksi] ubuncinane be-550 | 550 [79.8] |
Amandla oMzimba obuGqibeleleyo (N/mm2) [ksi] ubuncinane | 750 [108.8]] |
Ubude (%) ubuncinane | 25 |
Ukuqina (HBN) | 270max |
Ukucuthwa koMmandla oMnqamlezo (%) ubuncinane | 45 |
Impembelelo ye-Charpy V-notch kwi-ambient Temp (J) [ft.lb] | 80min [59min] |
Charpy V-notch Impact ku -46°C (J) [ft.lb] | 45av, 35min [33av, 25.8min] |