Imile, iFlethi, isikwere, iRound, iFine, iPlated kunye neBare Wire ASTM A167, AMS 5523
Isicelo
Amalungu eziko
IziTshintshiso zoBubushushu
Izixhobo zokugaya iPhepha
Izahlulo zokuPhuma kwiiTurbine zegesi
Amacandelo eNjini yeJet
Izixhobo zokucoca i-oyile
IKhemistri eqhelekileyo
Ikhabhoni | 0.080 ubuninzi |
IManganese | 2.00 ubuninzi |
Isilicon | 0.75 ubuninzi |
Chromium | 24.00- 26.00 |
Nickel | 19.00- 22.00 |
Molybdenum | 0.75 ubuninzi |
Iphosphorus | 0.040 ubuninzi |
Iipropati Zomzimba
Ukuxinana | 0.29 lbs/in³ 9.01 g/cm³ |
Ukuxhathisa koMbane | i-microhm-in (microhm-cm) |
68°F (20°C) | 37.0 (94.0) |
Ubushushu obuthile | I-BTU/lb/°F (kJ/kg•K) |
32-212°F (0-100°C) | 0.12 (0.50) |
I-Thermal Conductivity | BTU/iyure/ft²/ft/°F (W/m•K) |
Kwi-212°F (100°C) | 8.0 (13.8) |
Kwi-932°F (500°C) | 10.8 (18.7) |
I-Coefficient yeMean yoKwandiswa kweThermal | kwi/ku/°F (μm/m•K) |
32-212°F (0-100°C) | 8.0 x 10 (14.4) |
32-600°F (0-315°C) | 9.3 x 10 (16.7) |
32-1000°F (0-538°C) | 9.6 x 10 (17.3) |
32-1200°F (0-649°C) | 9.7x 10 (17.5) |
Imodyuli yeElasticity | I-KSI (MPa) 29.0 x 10³ (200 x 10³) kuxinzelelo 11.2 x 10³ ( 78 x 10³) kwi-torsion |
IMagnetic Permeability | H = 200 Oersteds |
I-Anealed | < 1.02 max |
Uluhlu olunyibilikayo | °F (°C) 2550 – 2650 (1399 – 1454) |
Iipropati zoomatshini
IiPropati zoomatshini kuBubushushu beGumbi
IIPROPATI | IQINISEKIWE |
Ukomelela kokugqibela kokuqina | 75 KSI min (515 MPA min) |
Amandla eSivuno (0.2% offset) | 30 KSI min (205 MPA min) |
Ukwandisa | 40% min Ubulukhuni Rb 95 max |
Iipropati | Ubushushu be-310S bunokubonelelwa kwiimeko ezahlukeneyo zobushushu. |
Qhagamshelana ne-Ulbrich Technical Service ngeenkcukacha.
Ukunyangwa kokuMhlwa
Jonga kwi-NACE (uMbutho weSizwe weeNjineli zeCorrosion) ukuze ufumane iingcebiso.
IiProperties Tempered Alloy 310S zinokuqengqeleka ukubanda ukufikelela kwiipropati zobushushu ezifunwa ngabathengi abathile kunye/okanye iimfuno zokuvelisa. Qhagamshelana ne-Ulbrich Wire ngeenkcukacha.
Iifom
Iikhoyili eziqhubekayo Sika ubude ukuya kubude Ukusika ngokuchanekileyo
ICold Forming Alloy 310S ine-ductility elungileyo kwaye inokuqengqeleka yenziwe, isitampu kwaye izotywe ngokulula.
I-Heat Treatment Alloy 310S inokuqiniswa kuphela ngokusebenza okubandayo.
Ukuwelda Ukufumana iziphumo ezingcono bhekisa ku: SSINA's “Ukuwelda kweziNtsimbi ezingatyiwayo kunye nokunye ukuDityaniswa
Iindlela”.
Unyino lweTyala kunye neDisclaimer of Warranty: Akukho mcimbi uya kuthi i-Ulbrich Stainless Steels kunye neSpecial Metals, Inc., ibe noxanduva lwawo nawuphi na umonakalo ovela kusetyenziso lolwazi olubandakanyiweyo kolu xwebhu okanye lufanelekile 'kwizicelo' eziphawulweyo. Sikholelwa ukuba ulwazi kunye nedatha enikiweyo ichanekile ngokona sinako kolwazi lwethu kodwa, yonke idatha ithathwa njengexabiso eliqhelekileyo kuphela. Yenzelwe ireferensi kunye nolwazi oluqhelekileyo kwaye ayikhuthazwa ukuba ichaze, uyilo okanye iinjongo zobunjineli. I-Ulbrich ithatha iwaranti echaziweyo okanye ecacileyo malunga nokudalwa okanye ukuchaneka kwedatha enikwe kolu xwebhu.