Imvula Ukuqinisa intsimbi engatyiwayo

  • I-17-4PH iPhepha leDatha leMathiriyeli

    Izazisi zamazwe ngamazwe

    AISI 630, ASTM A564-89 17-4PH, JIS SCS24 / SUS630, AFNOR Z7CNU15-05 / Z7CNU17-04

  • Imvula Ukuqinisa intsimbi engatyiwayo

    Ubushushu obuphezulu Ingxubevange yemichiza iBanga C Si Mn SP Cr Ni Mo Cu Nb Al enye ayikho ngaphezu kwe-0Cr17Ni4Cu4Nb 0.07 1 1 0.035 0.03 15.5~17.5 3~5 - 3~5 0.15~Cr01-7070. 035 0.03 16~18 6.5~7.5 - ≤0.5 - 0.75~1.5 - 0Cr15Ni7Mo2Al 0.09 1 1 0.035 0.03 14~16 6.5~7.75 2~3 - 0.75b-01C130Cuu 0.035 0.03 14–15.5 3.5~...