I-Hastelloy C-276 IINKCAZELO ZEDATHA ZOMTHETHO

Iinkcukacha zeMveliso

Iithegi zeMveliso

Ingcaciso yeMveliso

I-HT PIPE ibonelela nge-Hastelloy C276 Nickel alloy bar bar, i-Alloy C276 Bar umthengisi e-China. I-2.4819 bar ejikelezayo, intonga ye-Alloy C276, intonga ye-UNS N10276, i-Alloy C276 i-flat Bar, i-Hastelloy C276 ibha engenanto, i-Hastelloy C276 i-Nickel alloy round bar umthengisi, umthengisi wangaphandle.

IHastelloy C-276 (3)

Ziziphi iimpawu zeHastelloy C276?

● Ukumelana nokugqwesa okugqwesileyo ekunciphiseni okusingqongileyo
● Ukumelana okubalaseleyo nezinyibiliko eziqinileyo zeetyuwa ezineoxidizing, ezifana neferric kunye necupric chlorides.
● Iziqulatho ze-nickel eziphezulu kunye ne-molybdenum zibonelela ngokumelana ne-corrosion efanelekileyo ekunciphiseni okusingqongileyo
● Isiqulatho sekhabhoni esisezantsi esinciphisa imvula ye-carbide enomda weenkozo ngexesha le-welding ukugcina ukuxhathisa ukubola kwiindawo ezichatshazelwe bubushushu bamalungu adityanisiweyo.
● Ukumelana nokonakala kwendawo efana ne-pitting kunye noxinzelelo-i-corrosion cracking
● Esinye semathiriyeli embalwa ukumelana nokutyiwa kwerhasi yeklorin emanzi, i-hypochlorite kunye neklorin diokside.

I-Hastelloy C276 Nickel ialloy bar engqukuva Ukwakheka kwemichiza,%

Ni

Mo

Cr

Fe

W

Co

Mn

C

V

P

S

Si

Intsalela 15.0-17.0 14.5-16.5 4.0-7.0 3.0-4.5 2.5 ubuninzi 1.0 ubuninzi .01 ubuninzi .35 ubuninzi .04 ubuninzi .03 ubuninzi .08 ubuninzi

Iinkcukacha

Iimpawu zeASTM

Umbhobho Smls

Umbhobho Welded

Umbhobho Smls

Umbhobho Welded

Icwecwe/ipleyiti

Ibha

Ukuqulunqa

Ukulinganisa

Ucingo

B622 B619 B622 B626 B575 B574 B564 B366  

IHastelloy C276 Iipropati ezibonakalayo

Indawo yokunyibilika: 1325-1370 ℃

Ubuninzi: 8.90 g/cm3

Ingxubevange C276 Bar Mechanical Properties

Iimpawu zoomatshini I-tensile, min, ksi[MPa] Yield, min, ksi[MPa] Elongation, %(min)
IHastelloy C276 100[690] 41[283] 40

IiPropati zeTensile zeGumbi eziqhelekileyo zeMathiriyeli eAnealed

Ifom yeMveliso

I-Tensile (ksi)

.2% isivuno (ksi)

Elongation %

Ibha

110.0

52.6

62

Ipleyiti

107.4

50.3

67

Iphepha

115.5

54.6

60

Umbhobho kunye noMbhobho

105.4

45.4

70

INkcubeko yeNkampani

Iprospect yeNkampani: Iitarps kunye neCanvas Equipment eGqwesileyo Uphawu

Umnqophiso weNkampani: Yenziwe ngobulumko, inkampani yokugqibela, Yenza ixabiso eliphezulu kubathengi kunye nekamva elonwabisayo kunye nabasebenzi


  • Ngaphambili:
  • Okulandelayo:

  • Bhala umyalezo wakho apha kwaye uwuthumele kuthi